Page 1 of 1
Bridge refinish
Posted: Tue Jan 02, 2024 7:30 pm
by Patzag
My right hand rests on the bridge of my guitar while I play. After years of playing, the bridge has lost some of it's black anodizing and appears gray in spots.
I want to refinish it or at least darken the gray areas.
Any one here use this?
https://www.amazon.com/BW-Casey-Aluminu ... r=8-4&th=1
Re: Bridge refinish
Posted: Tue Jan 02, 2024 10:08 pm
by mmmguitar
+1 to Pat's request. And in case it's more than just my browser extensions preventing it from being displayed:
Here's the Amazon product he linked to. Based on the reviews, the product seems to be strictly for chemically dying fresh-cut, non-oxidized aluminum. Weren't the Fly bridges finished in a manner similar to powder-coating, but different due to the aluminum used? I'm afraid I don't recall the details. I know this matter was previously discussed on the old board; and hope someone remembers what the compromise ended up being when restoring the finish.
Edit: Gary (RIP) sanded down the worn spots on his bridge and refinished with matte black Duracoat gun finish:
viewtopic.php?p=4981#p4981
Re: Bridge refinish
Posted: Wed Jan 03, 2024 1:35 pm
by chrisandrews
I've repainted a few Parker bridges. They seem to be painted rather than anodised/Electro coated.
A dusting of etch primer, black base and satin topcoat will suffice. 2k topcoat is harder wearing
Hope that helps
Insta: @_the. captain_
Re: Bridge refinish
Posted: Wed Jan 03, 2024 3:06 pm
by Patzag
chrisandrews wrote: ↑Wed Jan 03, 2024 1:35 pm
A dusting if etch primer,
Thank you!
What does the above mean?
Re: Bridge refinish
Posted: Wed Jan 03, 2024 5:39 pm
by syncopa
Patzag wrote: ↑Wed Jan 03, 2024 3:06 pm
chrisandrews wrote: ↑Wed Jan 03, 2024 1:35 pm
A dusting if etch primer,
Thank you!
What does the above mean?
Here you go Pat
What does an etch primer do?
Etch Primers are single pack metal primers formulated with a combination of resins to maximise adhesion to the various metal surfaces on which they may be used. A low level of phosphoric acid is present in these primers to etch the metal surface and improve adhesion.